| US$500.00-750.00 | 1 Ton (MOQ) |
| Test Item | Testing Method | Standard | Test Result | Conclusion |
FILANENT DIAMETER | ISO1888 | 16±1um | 16.5 | pass |
| (Tex) ROVING LINEAR DENSITY | ISO1889 | 1200±60 | 1217 | pass |
| (% )MOISTURE CONTENT | ISO3344 | ≤0.1 | 0.04 | pass |
| (%) LOSS ON IGNITION | ISO3344 | 0.55±0.15 | 0.56 | pass |
| NET WEIGHT PER DOFF | ≥10kg | 18.7 | pass | |
| BREAKING STRENGTH | GB/T7689.5-2001 | ≥0.4 | 0.43 | pass |
| APPEARANCE | pass | |||
| REFERENCE STANDARD | GB/T18369---2001 | |||
| Test Item | Testing Method | Standard | Test Result | Conclusion |
| (tex) Roving Density | ISO1889 | 2400±120 | 2364 | pass |
| (%) Moisture Content | ISO3344 | ≤0.1 | 0.03 | pass |
| (%) Loss on Ignition | ISO1887 | 0.55±0.15 | 0.60 | pass |
| (μm) Filament Diameter | ISO1888 | 22±1 | 22.2 | pass |
| (N/tex) Tensile Strength | ISO3341 | ≥0.30 | 0.42 | pass |
Glass Type | GB/T 1549 | ECR | -- | pass |
Size Type | -- | Silan e | -- | pass |
APPEARANCE | pass | |||
Reference Standard | GB/T18369---2008 | |||
| Test Item | Testing Method | Standard | Test Result | Conclusion |
| (tex) Roving Density | ISO1889 | 4800±240 | 4778 | pass |
| (%) Moisture Content | ISO3344 | ≤0.1 | 0.03 | pass |
| (%) Loss on Ignition | ISO1887 | 0.50±0.15 | 0.64 | pass |
| (μm) Filament Diameter | ISO1888 | 25±1.0 | 25.2 | pass |
| (N/tex) Tensile Strength | ISO3341 | ≥0.30 | 0.45 | pass |
Glass Type | GB/T 1549 | ECR | -- | pass |
Size Type | -- | Silan e | -- | pass |
APPEARANCE | pass | |||
Reference Standard | GB/T18369---2008 | |||